The Impact of Electrolyte Additives in Lithium-ion Batteries Determined Using Isothermal Microcalorimetry
In this study, a high resolution TAM microcalorimeter equipped with 12 microcalorimeters was used to measure and quantitatively compare the heat flow of lithium-ion batteries that only vary in concentration of electrolyte additive.