View allAdhesives & SealantsAerospace / MilitaryAerospace, Military, & DefenseApplication NotesApplicationsArchiveARES G2 AccessoriesARES RheometerAutomated Density TesterAutomated Hardness TesterBatteriesBatteries & Battery MaterialsBatteriesBatteriesBiopharmaBiopharmaceuticalsBlog ApplicationsBlog Techniquescardiovascular instrumentsCase StudiesCeramicsCompositesCompositesDHR AccessoriesDifferential Scanning CalorimetersDifferential Scanning CalorimetryDIL 830 SeriesDilatometersDilatometryDilatometryDilatometryDiscovery Hybrid RheometersDraftsDynamic Mechanical Analysis (DMA)Dynamic Mechanical AnalyzersDynamic Mechanical Analyzers (DMA)Dynamic Mechanical Analyzers (Rheology)Dynamic Mechanical Analyzers (Thermal Analysis)ElastomersElectroForceElectroForceElectroForce NotesElectroForceElectroForceElectroForceElectronic Materials & ProductsElectronicsEnd of Life ProductsEngineered MaterialsFine & Specialty ChemicalsFlash Diffusivity SystemsFlash DiffusivityFlash DiffusivityFood ProductsGeneralGlass ProductsGuarded heat flow meterHeating MicroscopesHigh Pressure AnalyzersHigh Throughput DSCHorizontal DilatometersIn-Person TrainingInorganics - OtherInorganics - MineralsInsulation & Building MaterialsIsothermal CalorimetryIsothermal Titration CalorimetryLaser FlashLoad frame systemsMaterial CharacterizationMechanical TestingMechanical TestingMedical Device TestingMedical DevicesMedical DevicesMetals ProductsMicrocalorimetryMicrocalorimetryMicrocalorimetryMicrocalorimetryMicrocalorimetry NotesMicrocalorimetryMooney ViscometerMoving Die RheometerMulti-Specimen FatigueNews & InfoOils, Lubricants, & FluidsOptical DilatometersOptical FleximeterOrganic Chemicals & ProductsPaints, Inks, & CoatingsPaints, Inks, & CoatingsPercarbonatesPersonal Care & Household ProductsPetroleum ProductsPharmaceuticalsPharmaceuticalsPolymersPolymersprivateProduct videosProductsPromotionsQ SeriesQuenching DilatometersQuick start guidesRheologyRheologyRheologyRheology AccessoryRheologyRheology NotesRheologyRotational ViscometerRubberRubber AccessoriesRubberRubber Process AnalyzersRubberRubber TestingRubber TestingRubber TestingRubothermSeminarsService VideosSimultaneous Thermal AnalyzerSoftwareSoftwareTA Quick Talk VideosTech TipsTestbench and Planar Biaxial systemsTGA AccessoriesThermal AnalysisThermal AnalysisThermal AnalysisThermal Analysis NotesThermal AnalysisThermal ApplicationsThermal ConductivityThermal Conductivity & DiffusivityThermal Conductivity MeterThermal ConductivityThermal ConductivityThermogravimetric AnalysisThermomechanical AnalyzersThermophysical NotesThermophysical Properties NotesTrainingUncategorizedVapor Sorption AnalysisVertical DilatometersVideosDilatometryWebinarsMicrocalorimetryRheologyRubberThermal AnalysisXenon Flash

DIL 805L Quenching Dilatometers

The DIL805 Series comprises of four models: DIL 805L, DIL 805A are quenching dilatometers, DIL 805A/D is a quenching with the capability to deform the specimen by compression, and DIL 805A/D/T that can also stretch it in tension mode.

All four instruments are fully automated, self-contained units used to measure dimensional changes under extreme conditions of controlled heating and cooling.

Details

DIL 805A/D/T Quenching Dilatometers

The DIL805 Series comprises of four models: DIL 805L, DIL 805A are quenching dilatometers, DIL 805A/D is a quenching with the capability to deform the specimen by compression, and DIL 805A/D/T that can also stretch it in tension mode.

All four instruments are fully automated, self-contained units used to measure dimensional changes under extreme conditions of controlled heating and cooling.

Details

DIL 805A/D Quenching Dilatometers

The DIL805 Series comprises of four models: DIL 805L, DIL 805A are quenching dilatometers, DIL 805A/D is a quenching with the capability to deform the specimen by compression, and DIL 805A/D/T that can also stretch it in tension mode.

All four instruments are fully automated, self-contained units used to measure dimensional changes under extreme conditions of controlled heating and cooling.

Details

DIL 805A Quenching Dilatometers

The DIL805 Series comprises of four models: DIL 805L, DIL 805A are quenching dilatometers, DIL 805A/D is a quenching with the capability to deform the specimen by compression, and DIL 805A/D/T that can also stretch it in tension mode.

All four instruments are fully automated, self-contained units used to measure dimensional changes under extreme conditions of controlled heating and cooling.

Details

DIL 803 Dual Sample Dilatometer

To maximize sample throughput, DIL 803 and DIL 803L offers two-samples simultaneous operation. DIL803 and DIL 803L can also be operated with an inert reference sample for quasi-differential measurement, reducing the influence of measurement system expansion and increasing measurement accuracy under dynamic temperature conditions. The DIL 803 is designed for measurements under vacuum or inert gas while the DIL 803L is designed for measurements under air, making the DIL 803L ideally suited to measuring ceramic materials

Details

DIL 802 True Differential Dilatometer

For highest measurement accuracy, DIL 802 and DIL 802L provides a truly differential measurement. Measuring only the difference between the sample and the reference specimen, the True Differential design negates the influence of measurement system expansion on the sample measurement. This measurement design is of particular benefit for dynamic temperature programs such as those employed in Rate-Controlled-Sintering (RCS) and for measurements at lower temperatures. The DIL 802 is designed for measurements under vacuum or inert gas while the DIL 802L is designed for measurements under air.

Details

DIL 801 Single Sample Dilatometer

Suitable for a wide range of routine dilatometric tests, the DIL 801 and DIL 801L are horizontally configured single-sample dilatometers. The DIL 801 is designed for measurements under vacuum or inert gas while the DIL 801L is designed for measurements in air, making the DIL 801L ideally suited to measuring ceramic materials which are often processed in air.

Without a doubt DIL 801 and DIL 801L represent today the dilatometers with the best price / performance ratio on the market

Details

Differential Scanning Calorimetry Training

Applications Training:   DSC & Modulated DSC This lecture-based course covers theory applicable to all Differential Scanning Calorimeter (DSC) instruments (including previous generation instrument models), but is mainly designed around the Discovery instruments. The course will cover: Theory of operation Instrumentation Calibration Experimental Parameters Software operation Maintenance & Troubleshooting Applications Need help? If you are…

Details

Dielectric Thermal Analysis Accessory (DETA)

Dielectric Thermal Analysis Accessory (DETA) Extend the capabilities of your rheometer to measure dielectric properties from 20 Hz to 30 MHz. Description Features Technology Applications The ARES-G2 DETA is an accessory which expands the testing capability of the ARES-G2 rheometer to measure the response of materials by characterizing its capacitive and conductive properties. In dielectric…

Details

Dielectric Measurement

Dielectric Measurement Extends material characterization capabilities by providing an additional technique similar to dynamic mechanical. Description Technology Features Applications Dielectric Measurement The Dielectric Accessory extends material characterization capabilities by providing an additional technique similar to dynamic mechanical. In dielectric analysis, an oscillation electrical field (AC Field) is used as opposed to mechanical force (stress) and…

Details