DIL 803 Dual Sample Dilatometer
To maximize sample throughput, DIL 803 and DIL 803L offers two-samples simultaneous operation. DIL803 and DIL 803L can also be operated with an inert reference sample for quasi-differential measurement, reducing the influence of measurement system expansion and increasing measurement accuracy under dynamic temperature conditions. The DIL 803 is designed for measurements under vacuum or inert gas while the DIL 803L is designed for measurements under air, making the DIL 803L ideally suited to measuring ceramic materials