Sample Cutter
Sample preparation for RPA, MDR, and Mooney instruments is made safe and simple with the VS volumetric sample cutter. This dual-action pneumatic system allows for the preparation of uncured rubber specimens of a user-defined volume. Preparing samples in this well-controlled fashion reduces operational variability, greatly improving overall experimental precision.
The VS comes standard with a closing pressure of 6 bar. The sample is first compressed to the user-prescribed thickness, then cut to the die diameter. The closing pressure, and sample volume are user adjustable. Two handed operation and lateral guards guarantee safe operation at all times.
Details