Setting Up the Powder Flow Cell with Temperature Control on the DHR
Overview In this Tech Tip, we will show you how to set up the Powder Flow Cell with temperature control on the DHR.
DetailsSetting Up the Powder Shear Cell with Temperature Control on the DHR
Overview In this Tech Tip, we will show you how to setup up the powder shear cell with temperature control on the DHR.
DetailsSetting up the Ring on Plate Geometry on the Discovery HR for Tribo-Rheometry Testing
Overview Interested in measuring surface friction? TA Instruments Discovery Hybrid Rheometer offers four different tribo-rheometry accessories. This one, the ring-on-plate geometry, offers a surface to surface contact to measure surface friction. Rheometer users in the cosmetics, personal care, food, and electronics industries commonly use surface friction measurements to optimize their products. Watch this tech tip…
DetailsSetting Up the Saturator Reservoir for the Discovery SA
In this Tech Tip, we will set up the saturator reservoir for the Discovery SA.
DetailsShear Sandwich Clamp – DMA Q800
Q Series Trade-In The Q Series™ instruments will enter their End-of-Life at the end 2024. Repair and maintenance will be done on “best-effort” after 2024. However, it should be noted that our ability to make these repairs is subject to availability of parts. In the attempt to facilitate the transition to the current Discovery Series,…
DetailsShear Sandwich Clamp Installation & Calibration for the Discovery DMA 850
In this special TechTip Wednesday, we discuss the proper steps for installing and calibrating the shear sandwich clamp for the Discovery DMA 850 dynamic mechanical analyzer from TA Instruments!
Simple Determination of the Linear Viscoelastic Region of a Polymer Using a Rheometer
Materials such as polymers exhibit viscoelastic behavior which is directly related to molecular structure and formulation differences. To accurately evaluate the relationships between molecular structure and viscoelastic behavior requires that experiments, such as rheological measurements, be conducted in regions where the viscoelastic properties observed are independent of imposed stress or strain levels. That is, experiments must be conducted in the linear viscoelastic region.