View allAdhesives & SealantsAerospace / MilitaryAerospace, Military, & DefenseApplication NotesApplicationsArchiveARES AccessoriesARES RheometerAsphaltAutomated Density TesterAutomated Hardness TesterBatteriesBatteries & Battery MaterialsBatteriesBiopharmaBiopharmaceuticalsBlog ApplicationsBlog Techniquescardiovascular instrumentsCase StudiesCement & ConcreteCeramicsCompositesCompositesDeclarations of ConformityDHR AccessoriesDifferential Scanning CalorimetersDifferential Scanning CalorimetryDilatometersDilatometers Support DocumentsDilatometryDilatometryDilatometryDiscovery Hybrid RheometersDraftsDynamic Mechanical Analysis (DMA)Dynamic Mechanical AnalyzersDynamic Mechanical Analyzers (DMA)Dynamic Mechanical Analyzers (Rheology)Dynamic Mechanical Analyzers (Thermal Analysis)ElastomersElectroForceMechanical TestingElectroForce NotesElectroForceElectroForceElectroForceElectronic Materials & ProductsElectronicsEnd of Life ProductsEngineered MaterialsFilms & FibersFine & Specialty ChemicalsFlash Diffusivity SystemsFlash DiffusivityFlash DiffusivityFood ProductsGeneralGlass ProductsGuarded heat flow meterHigh Pressure AnalyzersHigh Throughput DSCHorizontal DilatometersIn-Person TrainingInorganics - OtherInorganics - MineralsInstallation GuidesInsulation & Building MaterialsIsothermal CalorimetryIsothermal Titration CalorimetryLaser FlashLoad frame systemsMaterial CharacterizationMechanical Testers Support DocumentsMechanical TestingMechanical TestingMedical Device TestingMedical DevicesMedical DevicesMetals ProductsMicrocalorimeters Support DocumentsMicrocalorimetryMicrocalorimetryMicrocalorimetryMicrocalorimetryMicrocalorimetry NotesMicrocalorimetryMooney ViscometerMoving Die RheometerMulti-Specimen FatigueNews & InfoOils, Lubricants, & FluidsOptical DilatometersOrganic Chemicals & ProductsPaints, Inks, & CoatingsPaints, Inks, & CoatingsPercarbonatesPersonal Care & Household ProductsPetroleum ProductsPharmaceuticalsPharmaceuticalsPolymersPolymersprivateProduct videosProductsPromotionsQ SeriesQuenching DilatometersQuick start guidesRheologyRheologyRheologyRheology AccessoryRheologyRheology NotesRheologyRheometers Support DocumentsRotational ViscometerRubberRubber AccessoriesRubberRubber Process AnalyzersRubberRubber TestingRubber TestingRubber TestingRubber Testing Support DocumentsRubothermSafety InformationSeminarsService VideosSimultaneous Thermal AnalyzerSoftwareSoftware Downloads SupportSoftwareSupportTA Quick Talk VideosTech TipsTestbench and Planar Biaxial systemsTGA AccessoriesThermal AnalysisThermal AnalysisThermal AnalysisThermal Analysis NotesThermal AnalysisThermal Analyzers Support DocumentsThermal ApplicationsThermal ConductivityThermal Conductivity & DiffusivityThermal Conductivity MeterThermal Conductivity Support DocumentsThermal ConductivityThermal ConductivityThermogravimetric AnalysisThermomechanical AnalyzersThermophysical NotesThermophysical Properties NotesTrainingUncategorizedVapor Sorption AnalysisVertical DilatometersVideosDilatometryWebinarsMicrocalorimetryRheologyRubberThermal AnalysisXenon Flash

What is Thermal Analysis?

Thermal analysis is a branch of material science that studies how a material’s properties change with temperature. From safe medicines to durable airplanes, countless products are made possible through thermal analysis. Understanding a material’s behavior under different temperatures is crucial for the successful design, processing, end use, and recyclability of completed products.

Details

When to Measure Glass Transition Temperature (Tg) on DSC, TMA, or DMA

The glass transition temperature (Tg) is a fundamental material property for defining material integrity, manufacturing conditions, and operating guidelines across applications such as polymers, electronics, and advanced materials.

Details

Fast Frequency Chirps vs Traditional Frequency Sweep Rheology

If your materials change during testing — curing, gelling, or cross‑linking — traditional step‑by‑step frequency measurements are not fast enough to keep up with rapidly changing properties. Fast frequency chirps offer the same data up to ten times faster than traditional frequency sweeps.

Details

Stronger, Lighter, Faster: Lightweighting in Aerospace Engineering with Material Characterization

The aerospace industry is embracing a growing trend toward lightweighting: using lower density materials without sacrificing mechanical strength, durability, or performance. Lightweighting offers numerous benefits, including accelerated production speed, increased energy efficiency, and improved recyclability.

Details

4 Characteristics of Real High-Force DMA and Why They Matter

While many instruments can measure DMA type properties (phase, tan delta, etc), many are not performing ‘real’ DMA experiments. On the surface, Dynamic Mechanical Analysis seems straightforward: apply periodic stress/strain and measure the sample’s mechanical response including the phase relationship, revealing characteristics like stiffness (storage modulus) and damping (loss modulus).

Details

What is Time Temperature Superposition, and Why is it Useful?

Developing high-performance materials for demanding applications requires predicting their behavior over a wide range of time scales. Rheology and DMA are powerful tools to understand and predict viscoelastic behavior, including how materials will respond to sudden forces or years of continuous use.

Details

Optimizing Thermal Interface Materials (TIMs) for Electronics: How TA Instruments Supports Advanced Thermal Management

As electronic devices grow more powerful and compact, thermal management has become a critical design challenge. Central to this challenge are Thermal Interface Materials (TIMs)—specialized materials engineered to enhance heat transfer between high-power electronic components and heat-dissipating surfaces.

Details

Polymer Rheology: Unlocking Insights with the Hybrid Rheometer

Polymer rheology plays a critical role in understanding the flow behavior and viscoelastic properties of polymers across the supply chain. Whether in polymer manufacturing, compounding, conversion, or recycling, precise rheological measurements are essential for optimizing processing conditions, ensuring product quality, and preventing defects.

Details

Why Rheology is Relevant and Accessible: Dispelling 5 Myths About Rheology

Will your paint stick to the wall or drip off? Does your low-fat cream cheese have the same texture as a full-fat version? How will new ingredients affect your formulation’s texture and application, especially as environmental conditions change? Rheology offers invaluable insights that help researchers, developers, and engineers across numerous industries optimize their products for performance and customer satisfaction.

Details