adt

ADT

Automated Density Tester

Density testing is made simple with the TA Instruments fully Automated Density Tester.

View brochure Contact Us

Sales Promotions

Density testing is made simple with the TA Instruments fully Automated Density Tester. This fully programmable, automated system measures the density of cured rubber materials using the finite difference (buoyancy) method. Active measurement of the fluid temperature increases accuracy by accounting for small changes in the density of the immersion fluid with temperature.

Test Method Finite Difference (buoyancy)
ISO 2781
ASTM D1817

Sample diameter

30 – 45 mm

Sample thickness

3 – 6 mm

Measurement range

< 1.0 g/cm3 to 2.5 g/cm3

Autosampler capacity

20
30 (optional)

Fluid Temperature Measurements

Standard

PRECISION DENSITY MEASUREMENT

ADT-circle

The finite difference method for density measurement relies on the measurement of sample weight dry, and immersed in a fluid, usually water. The difference between the dry and immersed weight is used with the known density of the fluid to calculate the volume of the specimen to a high degree of accuracy, irrespective of geometry.

A double gripper and carriage system is used to guarantee that dry weight values are entirely uninfluenced by system moisture or cross-contamination. Each sample is fully wetted by a user-defined number of separate immersions prior to immersed-mass measurement. This prevents error brought about by incomplete wetting and improves both accuracy and precision.

WALK-AWAY AUTOMATION

AHT-cirlce

Sequential, reliable, and unattended density measurements are made using an automatically fed sample tray with 20 or 30 sample capacity. This true walk-away automation is enhanced with software- driven test set-up, data collection, and pass/fail criteria.

Description

Density testing is made simple with the TA Instruments fully Automated Density Tester. This fully programmable, automated system measures the density of cured rubber materials using the finite difference (buoyancy) method. Active measurement of the fluid temperature increases accuracy by accounting for small changes in the density of the immersion fluid with temperature.

Specifications
Test Method Finite Difference (buoyancy)
ISO 2781
ASTM D1817

Sample diameter

30 – 45 mm

Sample thickness

3 – 6 mm

Measurement range

< 1.0 g/cm3 to 2.5 g/cm3

Autosampler capacity

20
30 (optional)

Fluid Temperature Measurements

Standard

Technology

PRECISION DENSITY MEASUREMENT

ADT-circle

The finite difference method for density measurement relies on the measurement of sample weight dry, and immersed in a fluid, usually water. The difference between the dry and immersed weight is used with the known density of the fluid to calculate the volume of the specimen to a high degree of accuracy, irrespective of geometry.

A double gripper and carriage system is used to guarantee that dry weight values are entirely uninfluenced by system moisture or cross-contamination. Each sample is fully wetted by a user-defined number of separate immersions prior to immersed-mass measurement. This prevents error brought about by incomplete wetting and improves both accuracy and precision.

Automation Options

WALK-AWAY AUTOMATION

AHT-cirlce

Sequential, reliable, and unattended density measurements are made using an automatically fed sample tray with 20 or 30 sample capacity. This true walk-away automation is enhanced with software- driven test set-up, data collection, and pass/fail criteria.

Videos