Time Dependent Stability of Aqueous Based Anode Slurries with Bio-Derived Binder by Rheological Methods
This application note will investigate the slurry aging and stability through its flow behavior and viscoelastic properties by using rheological methods. The slurry studied demonstrates a decrease in stability over time, which can be used to indicate the appropriate batch lifetime in a production environment.