Dynamic Mechanical Analysis (DMA)
Dynamic Mechanical Analysis (DMA) True axial DMA capability in bending, tension, and compression. Description Features Applications Axial Bending, Tension and Compression With its unique Force Rebalance Transducer (FRT), the ARES-G2 rheometer is the only rotational rheometer capable of performing linear Dynamic Mechanical Analysis (DMA) on solids in bending, tension and compression. Axial sample deformation is…