Furnaces for 80x and 80xL Series
Temperature Range -160°C to 700°C* RT to 1350°C RT to 1500°C RT to 1700°C
Heating Element NiCr with sheath with LN2cooling CrAIFe SiC Nobel Metal
Furnace Atmposphere Air Air Air Air
Thermocouple Type K S S B
Max. Heating Rate (K min-1) 50 50 50 25
Max. Cooling Rate (K min-1) 25 10 15 5
Temp. Profile Over 50 mm ± 2°C ± 3°C ± 5°C ± 5°C
Furnace Cooling Air Air Water Air

 