環氧樹脂的粉體流變分析:溫度對流動與剪切特性的影響
TA Instruments Powder Rheology Accessory for Temperature Control is used to study a filled epoxy resin for powder coatings. The results show that care must be taken in storage and processing, even at temperatures below the glass transition due to the effects on flowability and cohesion.