Inkbit and Waters Materials Sciences

Validating a New Class
of High-Performance Digital Materials

When a customer’s chosen epoxy failed at a lower stress load than expected, Inkbit set out to create a more durable, functional material to suit their industrial application. See how the TA Instruments Electroforce Apex 1 helped them engineer a higher-performing digital material in just six months.

Diagnose a real-world part failure with tensile and DMA temperature testing

Screen seven material formulations without lab-scale reformulation

Verify strength, stiffness, and fatigue life at true end-use temperatures

Move from failure analysis to a qualified, production-ready material

Access the Case Study

WHAT YOU WILL LEARN

Inside the Case Study

A field-failure investigation, told through the actual test data, from root-cause analysis to a qualified replacement material.

Diagnose the Failure

See how tensile testing at 23 °C, 50 °C, and 70 °C, paired with a DMA temperature sweep, pinpointed why a functional epoxy part failed below its rated stress load.

Screen Materials, Not Formulations

Learn how blending two compatible base resins directly on the printer let the team iterate through multiple digital material designs without benchtop research.

Test Under Real Conditions

Follow how five candidate materials were narrowed down using tensile strength, heat deflection, and DMA storage modulus data at true application temperatures.

Confirm with Fatigue Data

Review cyclic load testing from 95-950N that separated the final candidates and confirmed improved fatigue strength over the original material.

WHO THIS PAPER IS FOR

Built for Teams Engineering Custom Materials

Whether you’re formulating, printing, or qualifying materials for end-use parts, this case study maps directly to your workflow.

MATERIALS ENGINEERS

Additive Manufacturing & Polymers

See a repeatable framework for screening digital material formulations and correlating thermal transitions to real mechanical performance.

R&D TEAMS

Application Development

Understand how to move from a field failure to a qualified material candidate in months rather than years.

LAB MANAGERS

Test Lab & Equipment Planning

Evaluate how consolidating tensile, thermal, and fatigue testing onto one instrument simplifies installation, training, and daily operation.

Get the Full Case Study

Download «Validating a New Class of Digital Materials» to see the complete stress-strain data, DMA curves, and fatigue results behind Inkbit’s new epoxy digital material.