TA Instruments Introduces the New TAM IV Micro XL isothermal microcalorimeter
New Castle, Delaware, March 2, 2020 – TA Instruments announced today the introduction of the TAM IV Micro XL, a powerful isothermal microcalorimeter (IMC) specifically designed to measure the smallest electrochemical reactions inside battery cells. Outfitted with a large test chamber, this instrument allows scientists and engineers fabricate custom sized battery holders to accommodate battery…