AHT – Automated Hardness Tester
The AHT Automated Hardness Tester streamlines the measurement of Shore A hardness for cured rubber materials. This fully programmable, automated system measures the hardness of cured rubber materials according to all international standards for Shore A hardness. Each measurement involves the determination of a user-defined number of single point Shore A values. The individual readings, mean and median of this set are reported for each sample.
Details