Rheological Analysis of Hydrogel Materials
A rheometer is a powerful instrument that can be used to monitor the gel formation and also to measure the gel strength. Two case studies are discussed regarding the use of a TA Instruments’ rotational rheometer to analyze the properties of different types of hydrogels.