Micromechanical Multicyclic Creep Tests of Human Cortical Bone
This study had a threefold purpose: 1) study the creep response of bone to repetitive phsyiologically-relevant loading 2) to perform these types of tests on a small scale; and, 3) to illustrate and identify age-related effects on the mechanical properties of bone.