| ASTM |
A1033 |
Standard Practice for Quantitative Measurement and Reporting of Hypoeutectoid Carbon and Low-Alloy Steel Phase Transformations |
|
Dilatometry |
| ASTM |
C177 |
Standard Test Method for Steady-State Heat Flux Measurements and Thermal Transmission Properties by Means of the Guarded-Hot-Plate Apparatus |
|
Thermal Conductivity |
| ASTM |
C186 |
Standard Test Method for Heat of Hydration of Hydraulic Cement |
|
Isothermal Microcalorimetry |
| ASTM |
C335 |
Standard Test Method for Steady-State Heat Transfer Properties of Pipe Insulation |
|
Thermal Conductivity |
| ASTM |
C518 |
Standard Test Method for Steady-State Thermal Transmission Properties by Means of the Heat Flow Meter Apparatus |
|
Thermal Conductivity |
| ASTM |
C531 |
Standard Test Method for Linear Shrinkage and Coefficient of Thermal Expansion of Chemical-Resistant Mortars, Grouts, Monolithic Surfacings, and Polymer Concretes |
|
Dilatometry |
| ASTM |
C714 |
Standard Test Method for Thermal Diffusivity of Carbon and Graphite by Thermal Pulse Method |
|
Thermal Diffusivity |
| ASTM |
C824 |
Standard Practice for Specimen Preparation for Determination of Linear Thermal Expansion of Vitreous Glass Enamels and Glass Enamel Frits by the Dilatometer Method |
|
Dilatometry |
| ASTM |
C1046 |
Practice for In-Situ Measurement of Heat Flux and Temperature on Building Envelope Components |
|
Thermal Conductivity |
| ASTM |
C1679 |
Standard Practice for Measuring Hydration Kinetics of Hydraulic Cementitious Mixtures Using Isothermal Calorimetry |
|
Isothermal Microcalorimetry |
| ASTM |
C1702 |
Standard Test Method for Measurement of Heat of Hydration of Hydraulic Cementitious Materials Using Isothermal Conduction Calorimetry |
|
Isothermal Microcalorimetry |
| ASTM |
C1784 |
Standard Test Method for Using a Heat Flow Meter Apparatus for Measuring Thermal Storage Properties of Phase Change Materials and Products |
|
Thermal Conductivity |
| ASTM |
D6 |
Standard test method for loss on heating of oil and asphaltic compounds |
|
Thermogravimetric Analysis |
| ASTM |
D412 |
Elastomer and rubber testing: Standard Test Methods for Vulcanized Rubber and Thermoplastic Elastomers—Tension |
Medical Devices |
Load Frame Instruments |
| ASTM |
D430 |
Standard Test Methods for Rubber Deterioration—Dynamic Fatigue |
Medical Devices |
Load Frame Instruments |
| ASTM |
D618 |
Standard Practice for Conditioning Plastics for Testing |
|
Dynamic Mechanical Analysis |
| ASTM |
D696 |
Standard test method for coefficient of linear thermal expansion of plastics between -30 and 30°C with a vitreous silica dilatometer |
|
Dilatometry, Thermomechanical Analysis |
| ASTM |
D1329 |
Standard Test Method for Evaluating Rubber Property—Retraction at Lower Temperatures (TR Test) |
|
Rubber Testing |
| ASTM |
D1509 |
Standard test method for Carbon black - heating loss |
|
Thermogravimetric Analysis |
| ASTM |
D1646 |
Standard Test Methods for Rubber—Viscosity, Stress Relaxation, and Pre-Vulcanization Characteristics (Mooney Viscometer) |
|
Rubber Testing |
| ASTM |
D1647 |
Standard Test Methods for Rubber—Viscosity, Stress Relaxation, and Pre-Vulcanization Characteristics (Mooney Viscometer) |
|
Rubber Testing |
| ASTM |
D1817 |
Standard Test Method for Rubber Chemicals—Density |
|
Rubber Testing |
| ASTM |
D2196 |
Standard Test Methods for Rheological Properties of Non-Newtonian Materials by Rotational Viscometer |
|
Rheometry |
| ASTM |
D2216 |
Standard test method fof laboratory determination of water (moisture) content of soil and rock |
|
Thermogravimetric Analysis |
| ASTM |
D2240 |
Standard Test Method for Rubber Property—Durometer Hardness |
|
Rubber Testing |
| ASTM |
D2556 |
Standard Test Method for Apparent Viscosity of Adhesives Having Shear-Rate-Dependent Flow Properties Using Rotational Viscometry |
|
Rheometry |
| ASTM |
D2595 |
Standard test method for evaporation loss of lubricating greases over wide temperature range |
|
Thermogravimetric Analysis |
| ASTM |
D2832 |
Guide for determining volatile and nonvolatile content of paint and related coatings |
|
Thermogravimetric Analysis |
| ASTM |
D2866 |
Standard Test Method for Total Ash Content of Activated Carbon |
|
Thermogravimetric Analysis |
| ASTM |
D3172 |
Standard practice for proximate analysis of coal and coke |
|
Thermogravimetric Analysis |
| ASTM |
D3175 |
Standard test method for moisture in the analysis sample of coal and coke |
|
Thermogravimetric Analysis |
| ASTM |
D3418 |
Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetrye |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D3676 |
Standard Specification for Rubber Cellular Cushion Used for Carpet or Rug Underlay |
|
Rubber Testing |
| ASTM |
D3835 |
Standard Test Method for Determination of Properties of Polymeric Materials by Means of a Capillary Rheometer |
|
Rheometry |
| ASTM |
D3850 |
Standard Test Method for Rapid Thermal Degradation of Solid Electrical Insulating Materials By Thermogravimetric Method (TGA) |
|
Thermogravimetric Analysis |
| ASTM |
D3895 |
Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D4000 |
Standard Classification System for Specifying Plastic Materials |
|
Dynamic Mechanical Analysis |
| ASTM |
D4065 |
Plastics DMA: Standard Practice for Plastics: Dynamic Mechanical Properties: Determination and Report of Procedures |
Medical Devices |
Dynamic Mechanical Analysis,
High Force Dynamic Mechanical Analysis |
| ASTM |
D4066 |
Standard Practice for Plastics: Dynamic Mechanical Properties: Determination and Report of Procedures |
|
Dynamic Mechanical Analysis |
| ASTM |
D4092 |
Standard Terminology for Plastics: Dynamic Mechanical Properties |
|
Dynamic Mechanical Analysis, Rheometry, Rubber Testing |
| ASTM |
D4419 |
Standard Test Method for Measurement of Transition Temperatures of Petroleum Waxes by Differential Scanning Calorimetry (DSC) |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D4440 |
Dynamic Mechanical Testing on Polymer Melts |
Medical Devices |
Rheometry |
| ASTM |
D4473 |
Standard Test Method for Plastics: Dynamic Mechanical Properties: Cure Behavior |
|
Rheometry |
| ASTM |
D4535 |
Standard Test Methods for Measurement of Thermal Expansion of Rock Using Dilatometer |
|
Dilatometry |
| ASTM |
D4591 |
Standard test method for temperatures and heats of transition of fluoropolymers by Differential Scanning Calorimetry |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D4893 |
Standard test method for determination of pitch volatility |
|
Thermogravimetric Analysis |
| ASTM |
D5023 |
Standard Test Method for Plastics: Dynamic Mechanical Properties: In Flexure (Three-Point Bending) |
Medical Devices |
Dynamic Mechanical Analysis,
High Force Dynamic Mechanical Analysis |
| ASTM |
D5024 |
Compression |
Medical Devices |
Dynamic Mechanical Analysis,
High Force Dynamic Mechanical Analysis |
| ASTM |
D5026 |
Standard Test Method for Plastics: Dynamic Mechanical Properties: In Tension |
Medical Devices |
Dynamic Mechanical Analysis,
High Force Dynamic Mechanical Analysis |
| ASTM |
D5028 |
Standard test method for curing properties of pultrusion resins by thermal analysis |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D5279 |
Standard Test Method for Plastics: Dynamic Mechanical Properties: In Torsion |
Medical Devices |
Rheometry |
| ASTM |
D5289 |
Standard Test Method for Rubber Property—Vulcanization Using Rotorless Cure Meters |
|
Rubber Testing |
| ASTM |
D5418 |
Dual Cantilever Beam |
Medical Devices |
Dynamic Mechanical Analysis,
High Force Dynamic Mechanical Analysis |
| ASTM |
D5422 |
Standard Test Method for Measurement of Properties of Thermoplastic Materials by Screw-Extrusion Capillary Rheometer |
|
Rheometry |
| ASTM |
D5470 |
Standard Test Method for Thermal Transmission Properties of Thermally Conductive Electrical Insulation Materials |
|
Thermal Conductivity |
| ASTM |
D5483 |
Standard test method for oxidative induction time of lubricating greases by Pressure DSC |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D5515 |
Standard Test Method for Determination of the Swelling Properties of Bituminous Coal Using a Dilatometer |
|
Dilatometry |
| ASTM |
D5805 |
Standard Test Methods for Rubber—Determination of Carbon Black in Masterbatches |
|
Thermogravimetric Analysis |
| ASTM |
D5832 |
Standard Test Method for Volatile Matter Content of Activated Carbon Samples |
|
Thermogravimetric Analysis |
| ASTM |
D5885 |
Standard test method for oxidative induction time of polyolefin geosynthetics by Pressure DSC |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D5992 |
Rubber testing: Standard Guide for Dynamic Testing of Vulcanized Rubber and Rubber-Like Materials Using Vibratory Methods |
Medical Devices |
Dynamic Mechanical Analysis,
High Force Dynamic Mechanical Analysis |
| ASTM |
D6048 |
Standard Practice for Stress Relaxation Testing of Raw Rubber, Unvulcanized Rubber Compounds, and Thermoplastic Elastomers |
|
Rubber Testing |
| ASTM |
D6186 |
Standard test method for oxidative induction time of lubricating oils by Pressure DSC |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D6204 |
Standard Test Method for Rubber—Measurement of Unvulcanized Rheological Properties Using Rotorless Shear Rheometers |
|
Rubber Testing |
| ASTM |
D6370 |
Standard test method of rubber compositional analysis by TGA |
|
Thermogravimetric Analysis |
| ASTM |
D6375 |
Standard test method of evaporation loss of lubricating oils (NOACK) by TGA |
|
Thermogravimetric Analysis |
| ASTM |
D6382 |
Standard test method of DMA and TGA of roofing and waterproofing membrane materials |
|
Dynamic Mechanical Analysis, Thermogravimetric Analysis |
| ASTM |
D6559 |
Standard Test Method for Determination of Thermogravimetric (TGA) Air Reactivity of Baked Carbon Anodes and Cathode Blocks |
|
Thermogravimetric Analysis |
| ASTM |
D6580 |
Standard test method for determining metallic Zinc content in both Zinc dust pigment and in cured films of Zinc rich coatings by DSC |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D6601 |
Standard Test Method for Rubber Properties—Measurement of Cure and After-Cure Dynamic Properties Using a Rotorless Shear Rheometer |
|
Rubber Testing |
| ASTM |
D6602 |
Standard Practice for Sampling and Testing of Possible Carbon Black Fugitive Emissions or Other Environmental Particulate, or Both |
|
Thermogravimetric Analysis |
| ASTM |
D6604 |
Standard Practice for Glass Transition Temperatures of Hydrocarbon Resins by Differential Scanning Calorimetry |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D6744 |
Standard Test Method for Determination of the Thermal Conductivity of Anode Carbons by the Guarded Heat Flow Meter Technique |
|
Thermal Conductivity |
| ASTM |
D7028 |
Standard Test Method for Glass Transition Temperature (DMA Tg) of Polymer Matrix Composites by Dynamic Mechanical Analysis (DMA) |
|
Dynamic Mechanical Analysis |
| ASTM |
D7050 |
Standard Practice for Rubber from Natural Sources Sampling and Sorting Bales Based on Predicted Processing Properties
|
|
Rubber Testing |
| ASTM |
D7138 |
Standard Test Method to Determine Melting Temperature of Synthetic Fibers |
Composites, Polymers |
Differential Scanning Calorimetry |
| ASTM |
D7175 |
Standard Test Method for Determining the Rheological Properties of Asphalt Binder Using a Dynamic Shear Rheometer |
|
Rheometry |
| ASTM |
D7340 |
Standard Practice for Thermal Conductivity of Leather |
|
Thermal Conductivity |
| ASTM |
D7426 |
Standard Test Method for Assignment of the DSC Procedure for Determining Tg of a Polymer or an Elastomeric Compound |
Polymers |
Differential Scanning Calorimetry |
| ASTM |
D7582 |
Standard Test Methods for Proximate Analysis of Coal and Coke by Macro Thermogravimetric Analysis |
|
Thermogravimetric Analysis |
| ASTM |
D8059 |
ASTM 8059 Standard Test Method for Rubber Compounds-Measurement of Unvulcanized Dynamic Strain Softening (Payne Effect) Using Sealed Cavity Rotorless Shear Rheometers |
|
Rubber Testing |
| ASTM |
E8 |
Standard Test Methods for Tension Testing of Metallic Materials |
Medical Devices |
Load Frame Instruments |
| ASTM |
E228 |
Standard test method for coefficient of linear thermal expansion of solid materials with a push rod dilatometer |
|
Dilatometry |
| ASTM |
E359 |
Standard test method for chemical analysis of Soda Ash (Sodium Carbonate) |
|
Thermogravimetric Analysis |
| ASTM |
E466 |
Conducting Force Controlled Constant Amplitude Axial Fatigue Tests of Metallic Materials |
Medical Devices |
Load Frame Instruments |
| ASTM |
E473 |
Terminology relating to thermal analysis and rheology |
|
Dilatometry, Thermomechanical Analysis |
| ASTM |
E487 |
Standard test method for contant temperature stability of chemical materials |
|
Differential Scanning Calorimetry |
| ASTM |
E537 |
Standard test method for assessing the thermal stability of chemical by methods of thermal analysis |
|
Differential Scanning Calorimetry |
| ASTM |
E698 |
Standard test method for Arrhenius kinetic constants for thermally unstable materials using Differential Scanning Calorimetry and the Flynn/Wall/Ozawa Method |
|
Differential Scanning Calorimetry |
| ASTM |
E793 |
Test Method for Enthalpies of Fusion and Crystallization by Differential Scanning Calorimetry |
Medical Devices |
Differential Scanning Calorimetry |
| ASTM |
E794 |
Test Method for Melting and Crystallization Temperatures by Thermal Analysis |
Medical Devices |
Differential Scanning Calorimetry |
| ASTM |
E831 |
Test Method for Linear Thermal Expansion of Solid Materials by Thermomechanical Analysis |
Medical Devices |
Thermomechanical Analysis |
| ASTM |
E928 |
Standard test method for purity by Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
E967 |
Standard test method for temperature calibration of Differential Scanning Calorimeters and Differential Thermal Analyzers |
|
Differential Scanning Calorimetry |
| ASTM |
E968 |
Standard practice for heat flow calibration of Differential Scanning Calorimeters |
|
Differential Scanning Calorimetry |
| ASTM |
E1131 |
Test Method for Compositional Analysis by Thermogravimetry |
Medical Devices |
Thermogravimetric Analysis |
| ASTM |
E1142 |
Terminology relating to thermophysical properties |
|
Thermogravimetric Analysis |
| ASTM |
E1225 |
Standard Test Method for Thermal Conductivity of Solids Using the Guarded-Comparative-Longitudinal Heat Flow Technique |
|
Thermal Conductivity |
| ASTM |
E1231 |
Standard practice for calculation of hazard potential figures of merit for thermally unstable materials |
|
Differential Scanning Calorimetry |
| ASTM |
E1269 |
Standard test method for determining specific heat capacity by Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
E1356 |
Test Method for the Assignment of the Glass Transition Temperatures by Differential Scanning Calorimetry |
Medical Devices |
Differential Scanning Calorimetry |
| ASTM |
E1363 |
Standard test method for temperature calibration of Thermomechanical Analyzers |
|
Dilatometry, Thermomechanical Analysis |
| ASTM |
E1461 |
Standard Test Method for Thermal Diffusivity by the Flash Method |
|
Thermal Diffusivity |
| ASTM |
E1530 |
Standard Test Method for Evaluating the Resistance to Thermal Transmission of Materials by the Guarded Heat Flow Meter Technique |
|
Thermal Conductivity |
| ASTM |
E1545 |
Test Method for Assignment of a Glass Transition Temperature by Thermomechanical Analysis |
Medical Devices |
Thermomechanical Analysis |
| ASTM |
E1582 |
Standard practice for calibration of temperature scale for TGA |
|
Thermogravimetric Analysis |
| ASTM |
E1640 |
DMA testing: Standard Test Method for Assignment of the Glass Transition Temperature by Dynamic Mechanical Analysis |
Medical Devices |
Dynamic Mechanical Analysis,
High Force Dynamic Mechanical Analysis |
| ASTM |
E1641 |
Test Method for Decomposition Kinetics by Thermogravimetry Using the Flynn/Wall/Ozawa Method |
Medical Devices |
Thermogravimetric Analysis |
| ASTM |
E1782 |
Standard test method for determining vapor pressure by DSC and DTA |
|
Differential Scanning Calorimetry |
| ASTM |
E1824 |
Test Method for Assignment of a Glass Transition Temperature Using Thermomechanical Analysis: Tension Method |
Medical Devices |
Thermomechanical Analysis |
| ASTM |
E1842 |
Standard test method for assignment of the glass transition temperature by TMA in tension |
|
Dilatometry, Thermomechanical Analysis |
| ASTM |
E1858 |
Standard test method for oxidative induction time of hyrocarbons by Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
E1860 |
Standard test method for time base calibration of thermal analyzers |
|
Differential Scanning Calorimetry |
| ASTM |
E1867 |
Standard Test Method for Temperature Calibration of Dynamic Mechanical Analyzers |
|
Dynamic Mechanical Analysis |
| ASTM |
E1868 |
Standard test method for loss on drying by thermogravimetry |
|
Thermogravimetric Analysis |
| ASTM |
E1877 |
Standard test method for thermal endurance of materials from TGA decomposition |
|
Thermogravimetric Analysis |
| ASTM |
E1952 |
Standard test method for thermal conductivity and thermal diffusivity by Modulated Temperature Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
E1953 |
Descriptionn of thermal analysis apparatus |
|
Differential Scanning Calorimetry, Thermogravimetric Analysis |
| ASTM |
E1970 |
Statistical treatment of thermal analysis data |
|
Differential Scanning Calorimetry, Thermogravimetric Analysis |
| ASTM |
E2008 |
Standard Test Methods for Volatility Rate by Thermogravimetry |
|
Thermogravimetric Analysis |
| ASTM |
E2009 |
Standard test method for oxidative onset temperature of hydrocarbons by Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
E2040 |
Standard test method for mass scale calibration of TGA's |
|
Thermogravimetric Analysis |
| ASTM |
E2041 |
Standard test method for estimating kinetic parameters by Differential Scanning Calorimetry using the Borchardt and Danials method |
|
Differential Scanning Calorimetry |
| ASTM |
E2046 |
Standard test method for reaction induction time by Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
E2069 |
Standard test method for temperature calibration on cooling of DSC's |
|
Differential Scanning Calorimetry |
| ASTM |
E2070 |
Standard test method for kinetic parameters by Differential Scanning Calorimetry using isothermal methods |
|
Differential Scanning Calorimetry |
| ASTM |
E2092 |
Standard test method for distortion temperature in 3-point bending by TMA |
|
Dilatometry, Thermomechanical Analysis |
| ASTM |
E2105 |
Standard Practice for General Techniques of Thermogravimetric Analysis (TGA) Coupled With Infrared Analysis (TGA/IR) |
|
Thermogravimetric Analysis |
| ASTM |
E2113 |
Standard test method for length change calibrations of Thermomechanical Analyzers |
|
Dilatometry, Thermomechanical Analysis |
| ASTM |
E2160 |
Standard test method for heats of reaction by Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
E2253 |
Standard test method for enthalpy measurement vvalidation of Differential Scanning Calorimeters |
|
Differential Scanning Calorimetry |
| ASTM |
E2254 |
Standard Test Method for Storage Modulus Calibration of Dynamic Mechanical Analyzers |
|
Dynamic Mechanical Analysis |
| ASTM |
E2347 |
Standard Test Method for Indentation Softening Temperature by Thermomechanical Analysis |
|
Dilatometry, Thermomechanical Analysis |
| ASTM |
E2402 |
Standard test method for mass loss and residue measurement validation of TGA's |
|
Thermogravimetric Analysis |
| ASTM |
E2403 |
Standard test method of sulfated ash of organic materials by TGA |
|
Thermogravimetric Analysis |
| ASTM |
E2425 |
Standard Test Method for Loss Modulus Conformance of Dynamic Mechanical Analyzers |
|
Dynamic Mechanical Analysis |
| ASTM |
E2550 |
Test Method for Thermal Stability by Thermogravimetry |
Medical Devices |
Thermogravimetric Analysis |
| ASTM |
E2551 |
Standard Test Method for Humidity Calibration (or Conformation) of Humidity Generators for Use with Thermogravimetric Analyzers |
|
Thermogravimetric Analysis |
| ASTM |
E2585 |
Standard Practice for Thermal Diffusivity by the Flash Method |
|
Thermal Diffusivity |
| ASTM |
E2602 |
Standard Test Methods for the Assignment of the Glass Transition Temperature by Modulated Temperature Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
E2603 |
Standard Practice for Calibration of Fixed-Cell Differential Scanning Calorimeters |
|
Differential Scanning Calorimetry |
| ASTM |
E2712 |
Standard test method for determining specific heat capacity by Sinusoidal Modulated Temperature Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
E2769 |
Standard Test Method for Elastic Modulus by Thermomechanical Analysis Using Three-Point Bending and Controlled Rate of Loading |
|
Dilatometry, Thermomechanical Analysis |
| ASTM |
E2781 |
Standard Practice for Evaluation of Methods for Determination of Kinetic Parameters by Thermal Analysis |
|
Differential Scanning Calorimetry |
| ASTM |
E2918 |
Standard Test Method for Performance Validation of Thermomechanical Analyzers |
|
Dilatometry, Thermomechanical Analysis |
| ASTM |
E2923 |
Standard Practice for Longevity Assessment of Firestop Materials Using Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
F382 |
Bone plate testing - Standard Specification and Test Method for Metallic Bone Plates |
Medical Devices |
Load Frame Instruments |
| ASTM |
F384 |
Fracture fixation device testing - Standard Specifications and Test Methods for Metallic Angled Orthopedic Fracture Fixation Devices |
Medical Devices |
Load Frame Instruments |
| ASTM |
F543 |
Standard Specification and Test Methods for Metallic Medical Bone Screws |
Medical Devices |
Load Frame Instruments |
| ASTM |
F564 |
Bone staple testing - Standard Specification and Test Methods for Metallic Bone Staples |
Medical Devices |
Load Frame Instruments |
| ASTM |
F1264 |
Intramedullary device testing - Standard Specification and Test Methods for Intramedullary Fixation Devices |
Medical Devices |
Load Frame Instruments |
| ASTM |
F1440 |
Hip stem fatigue: Standard Practice for Cyclic Fatigue Testing of Metallic Stemmed Hip Arthroplasty Femoral Components Without Torsion |
Medical Devices |
Load Frame Instruments |
| ASTM |
F1717 |
Standard Test Methods for Spinal Implant Constructs in a Vertebrectomy Model |
Medical Devices |
Load Frame Instruments |
| ASTM |
F1781 |
Finger component testing - Standard Specification for Elastomeric Flexible Hinge Finger Total Joint Implants |
Medical Devices |
Load Frame Instruments,
TestBench and Planar Biaxial Instruments |
| ASTM |
F1798 |
Spinal construct fatigue: Standard Test Method for Evaluating the Static and Fatigue Properties of Interconnection Mechanisms and Subassemblies Used in Spinal Arthrodesis Implants |
Medical Devices |
Load Frame Instruments |
| ASTM |
F1800 |
Knee component fatigue - Standard Practice for Cyclic Fatigue Testing of Metal Tibial Tray Components of Total Knee Joint Replacements |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2004 |
Test Method for Transformation Temperature of Nickel-Titanium Alloys by Thermal Analysis |
Medical Devices |
Differential Scanning Calorimetry |
| ASTM |
F2077 |
Spinal construct fatigue: Test Methods for Intervertebral Body Fusion Devices |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2118 |
Standard Test Method for Constant Amplitude of Force Controlled Fatigue Testing of Acrylic Bone Cement Materials |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2193 |
Standard Specifications and Test Methods for Components Used in the Surgical Fixation of the Spinal Skeletal System |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2346 |
Spinal construct fatigue: Standard Test Methods for Static and Dynamic Characterization of Spinal Artificial Discs |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2477 |
Pulsatile stent testing: Standard Test Methods for in vitro Pulsatile Durability Testing of Vascular Stents |
Medical Devices |
Cardiovascular Test Instruments |
| ASTM |
F2516 |
Standard Test Method for Tension Testing of Nickel-Titanium Superelastic Materials |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2606 |
Stent testing: Standard Guide for Three-Point Bending of Balloon Expandable Vascular Stents and Stent Systems |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2624 |
Spinal construct fatigue: Standard Test Method for Static, Dynamic, and Wear Assessment of Extra-Discal Single Level Spinal Constructs |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2625 |
Standard Test Method for Measurement of Enthalpy of Fusion, Percent Crystallinity, and Melting Point of Ultra-High-Molecular Weight Polyethylene by Means of Differential Scanning Calorimetry |
|
Differential Scanning Calorimetry |
| ASTM |
F2722 |
Knee component testing - Standard Practice for Evaluating Mobile Bearing Knee Tibial Baseplate Rotational Stops |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2790 |
Spinal construct fatigue: Standard Practice for Static and Dynamic Characterization of Motion Preserving Lumbar Total Facet Prostheses |
Medical Devices |
Load Frame Instruments |
| ASTM |
F2942 |
Stent testing: Standard Guide for in vitro Axial, Bending, and Torsional Durability Testing of Vascular Stents |
Medical Devices |
Load Frame Instruments,
TestBench and Planar Biaxial Instruments |
| ASTM |
F3014 |
Standard Test Method for Penetration Testing of Needles Used in Surgical Sutures |
Medical Devices |
Load Frame Instruments,
TestBench and Planar Biaxial Instruments |
| ASTM |
F3140 |
Standard Test Method for Cyclic Fatigue Testing of Metal Tibial Tray Components of Unicondylar Knee Joint Replacements |
Medical Devices |
Load Frame Instruments |
| ASTM |
F3211 |
Standard Guide for Fatigue-to-Fracture (FtF) Methodology for Cardiovascular Medical Devices |
Medical Devices |
Multi-Specimen Fatigue,
Cardiovascular Test Instruments |
| ASTM |
F3268 |
Standard Guide for in vitro Degradation Testing of Absorbable Metals |
Medical Devices |
Cardiovascular Test Instruments |
| BS |
903-A58 |
Physical testing of rubber – Part A58: Methods using the Mooney viscometer. |
|
Rubber Testing |
| DIN |
53505 |
Shore A and Shore D Hardness Testing of Rubber (Shore A). |
|
Rubber Testing |
| DIN |
53523 |
Testing of Rubber and Elastomers; Testing with the Mooney Shearing Disk Viscometer; Determining the Scorching Behaviour |
|
Rubber Testing |
| DIN |
53529 |
Testing of rubber and elastomers; measurement of vulcanization characteristics (curometry); evaluation of cross-linking isotherms in terms of reaction kinetics |
|
Rubber Testing |
| ISO |
289 |
Rubber, unvulcanized — Determinations using a shearing-disc viscometer |
|
Rubber Testing |
| ISO |
527 |
Plastics — Determination of tensile properties |
Medical Devices |
Load Frame Instruments |
| ISO |
868 |
Plastics and ebonite — Determination of indentation hardness by means of a durometer (Shore hardness) |
|
Rubber Testing |
| ISO |
1099 |
Metallic materials — Fatigue testing — Axial force-controlled method |
Medical Devices |
Load Frame Instruments |
| ISO |
2781 |
Rubber, vulcanized or thermoplastic – Determination of density |
|
Rubber Testing |
| ISO |
5085 |
Textiles -- Determination of thermal resistance |
|
Thermal Conductivity |
| ISO |
5840 |
Heart valve testing: Cardiovascular Implants -- Cardiac Valve Prosthesis |
Medical Devices |
Cardiovascular Test Instruments |
| ISO |
6475 |
Implants for Surgery: Metallic Bone Screws |
Medical Devices |
Load Frame Instruments |
| ISO |
6502 |
Guide to the use of curemeters |
|
Rubber Testing |
| ISO |
6721-4, -5 |
Plastics — Determination of dynamic mechanical properties |
Medical Devices |
Dynamic Mechanical Analysis,
High Force Dynamic Mechanical Analysis |
| ISO |
7198 |
Cardiovascular implants and extracorporeal systems — Vascular prostheses — Tubular vascular grafts and vascular patches (NA for our equipment) |
Medical Devices |
Load Frame Instruments,
Cardiovascular Test Instruments |
| ISO |
7206 |
Implants for surgery — Partial and total hip joint prosthese |
Medical Devices |
Load Frame Instruments |
| ISO |
7619 |
Rubber, vulcanized or thermoplastic — Determination of indentation hardness |
|
Rubber Testing |
| ISO |
7800 |
Metal Wire Torsion Testing |
Medical Devices |
Load Frame Instruments |
| ISO |
8301 |
Thermal insulation -- Determination of steady-state thermal resistance and related properties -- Heat flow meter apparatus |
|
Thermal Conductivity |
| ISO |
8302 |
Thermal insulation -- Determination of steady-state thermal resistance and related properties -- Guarded hot plate apparatus |
|
Thermal Conductivity |
| ISO |
11357 |
Plastics -- Differential scanning calorimetry (DSC) |
|
Differential Scanning Calorimetry |
| ISO |
11358 |
Plastics -- Thermogravimetry (TG) of polymers |
Polymers |
Thermogravimetric Analysis |
| ISO |
11359 |
Plastics -- Thermomechanical analysis (TMA) |
|
Thermomechanical Analysis |
| ISO |
12106 |
Metallic materials — Fatigue testing — Axial-strain-controlled method |
Medical Devices |
Load Frame Instruments |
| ISO |
12988 |
Carbonaceous materials used in the production of aluminium -- Baked anodes -- Determination of the reactivity to carbon dioxide -- Part 2: Thermogravimetric method |
|
Thermogravimetric Analysis |
| ISO |
12989 |
Carbonaceous materials used in the production of aluminium -- Baked anodes and sidewall blocks -- Determination of the reactivity to air -- Part 2: Thermogravimetric method |
|
Thermogravimetric Analysis |
| ISO |
13145 |
Determination of viscosity and stress relaxation using a rotorless sealed shear rheometer |
|
Rubber Testing |
| ISO |
13787 |
Thermal insulation products for building equipment and industrial installations -- Determination of declared thermal conductivity |
|
Thermal Conductivity |
| ISO |
13826 |
Metallic and other inorganic coatings -- Determination of thermal diffusivity of thermally sprayed ceramic coatings by laser flash method |
|
Thermal Diffusivity |
| ISO |
14607 |
Non-active surgical implants — Mammary implants — Particular requirements |
Medical Devices |
Load Frame Instruments |
| ISO |
14630 |
Non-active surgical implants — General requirements |
Medical Devices |
ElectroForce Mechanical Testing |
| ISO |
14801 |
Dentistry — Implants — Dynamic loading test for endosseous dental implants |
Medical Devices |
Load Frame Instruments |
| ISO |
14879 |
Determination of endurance properties of knee tibial trays (Similar/same to ASTM F1800) |
Medical Devices |
Load Frame Instruments |
| ISO |
22007 |
Plastics -- Determination of thermal conductivity and thermal diffusivity |
|
Thermal Diffusivity |
| ISO |
25539 |
Cardiovascular implants -- Endovascular devices |
Medical Devices |
Multi-Specimen Fatigue,
Cardiovascular Test Instruments |
| ISO |
80369-20 |
Small-bore connectors for liquids and gases in healthcare applications — Part 20: Common test methods |
Medical Devices |
Load Frame Instruments |
| NF |
T46-052 |
Rubber, vulcanized or thermoplastic – Determination of indentation hardness – Part 1: durometer method (Shore hardness). |
|
Rubber Testing |
| NF |
T51-174 |
Plastics and ebonite – Determination of indentation hardness by means of a durometer shore hardness. |
|