Keywords: Dysphagia, Normal Force
RH163
Abstract
Dysphagia-oriented foods require careful mechanical characterization to ensure safe and effective swallowing. Traditional descriptors such as nectar, honey, and pudding have long been used to communicate consistency levels, but these terms do not guarantee equivalent flow behavior across products and must be interpreted within the context of modern International Dysphagia Diet Standardization Initiative (IDDSI) standards. This study evaluates three model formulations representing these consistency levels using a combination of steady shear, oscillatory, axial stress, and tack/extensional measurements. The results reveal a clear progression in viscosity, elasticity, structural strength, and cohesiveness from nectar to honey to pudding. Axial stress measurements highlight differences in flow-induced structural anisotropy, while tack tests demonstrate increasing extensional resistance and cohesive integrity. Together, these measurements show that mechanical descriptors beyond viscosity, particularly those related to structural strength and deformation resistance, provide valuable insight into the functional performance of dysphagia-oriented foods. The findings support the use of normal-force-related measurements as complementary parameters for characterizing bolus behavior under conditions relevant to swallowing.
The modification of food and liquid consistency is a central strategy in dysphagia management. Historically, the terms nectar, honey, and pudding have been used to describe three broad levels of thickness within the National Dysphagia Diet (NDD). In the current IDDSI framework, these categories broadly correspond to Level 2 (Mildly Thick), Level 3 (Moderately Thick), and Level 4 (Extremely Thick/Purée). However, because legacy terminology does not ensure consistent flow behavior across products, IDDSI testing remains essential for accurate classification.
Thickened liquids are widely used because increasing consistency generally slows bolus flow, which may improve airway protection [1]. At the same time, excessive thickness can increase oral or pharyngeal residue and reduce patient acceptability. As a result, understanding the mechanical behavior of dysphagiaoriented foods requires a multidimensional approach that goes beyond viscosity alone.
Swallowing involves more than shear flow. The bolus is compressed, stretched, and deformed during oral and pharyngeal transit. Mechanical descriptors such as cohesiveness, structural integrity, and resistance to deformation therefore play a critical role in determining functional performance. This application note examines three model formulations — nectar, honey, and pudding — to explore how their rheological properties relate to their expected behavior during swallowing.
All rheological tests were performed on a TA Instruments™ Discovery™ Hybrid Rheometer (HR) 30 at 25 °C using a smooth 40 mm parallel‑plate geometry. The following protocols were applied:
Strain Sweep (1 Hz, 0.1%–10,000%)
This test evaluates the structural integrity of the samples by determining the strain at which the storage modulus (G′) and loss modulus (G″) intersect. The crossover point provides insight into the deformation tolerance and network strength of each formulation.
Steady-State Flow Sweep (0.1–500 s-1)
This test characterizes viscosity as a function of shear rate, revealing shear-thinning behavior and differences in flow resistance across the three formulations.
Tack Test (Normal Separation at 100 μm/s)
The tack test measures the force required to separate the plates, providing information about:
- adhesion work
- extensional resistance
- cohesive failure behavior
- and the ability of the material to maintain structural integrity during elongation.
Normal Stress Monitoring
Axial stress was recorded during shear flow to assess how each formulation responds to deformation in the normal direction. This parameter reflects differences in structural anisotropy and cohesiveness under flow.
Three model dysphagia formulations were prepared to mimic the standard consistency levels commonly used in the food industry for patients with swallowing disorders: nectar, honey, and pudding. These samples were designed to provide a gradual increase in viscosity, elasticity, and structural strength. The nectar sample corresponds to the least structured system, the honey sample represents an intermediate level of consistency and cohesiveness, and the pudding sample corresponds to the most structured, gel-like material. The use of these three model systems allows a comparative evaluation of the relationship between consistency and rheological performance.
The shape of the debonding curves suggests important differences in failure mechanism among the three materials. The broader and more sustained stress decay observed for pudding in Figure 1 indicates that, after the peak, the sample was still able to support load over a wide deformation range. This behavior is consistent with a highly cohesive and structured network that fails progressively rather than abruptly. Honey followed the same trend, although at lower stress levels, confirming an intermediate degree of extensional stability. In contrast, nectar showed a much lower peak and a narrower curve, suggesting a weaker internal network and a reduced ability to maintain cohesive bridges during plate separation.
The combined results of viscosity in Figure 2 and normal force in Figure 1 show that increasing consistency is associated not only with higher viscosity, but also with greater resistance to extensional breakup. From a functional perspective, stronger tack behavior may help preserve bolus integrity during handling and swallowing. However, excessive cohesion may also increase the effort required for oral processing.
The normal force data in Figure 2 revealed a progressive increase in normal-stress development from nectar to honey to pudding. While all samples were shear-thinning, pudding and honey generated substantially higher positive axial forces at medium and high shear rates, indicating stronger flow-induced elastic anisotropy and greater bolus cohesiveness.
- Swallowing involves more than shear flow; the bolus is also compressed, stretched, and deformed during oral and pharyngeal transit [2].
- Normal forces provide information about bolus cohesiveness and structural integrity under flow.
- They help distinguish formulations that may show similar viscosity but different elastic behavior.
- They reflect a functional balance between improved bolus integrity and increased resistance to deformation.



Table 1. Relevant values extracted from the rheological experiments
| Sample/Parameter | Nectar | Honey | Pudding |
|---|---|---|---|
| Max Normal Stress (Pa) | 210 | 690 | 1015 |
| Adhesion work (microJ) | 454 | 690 | 1250 |
| Crossover Strain (%) | 247 | 183 | 103 |
| Crossover Stress (Pa) | 15.6 | 52.8 | 63.1 |
Overall, the results suggest a clear functional ranking (Table 1). From the stress sweeps showed in Figure 3 we can conclude that nectar appears to offer the lowest resistance to flow and deformation, which may make oral transfer easier but provides the least structural support. On the top of that, nectar exhibited the lowest crossover modulus, indicating the least stiff structure at the G′/G′′ crossover. At the same time, it showed the highest crossover strain, suggesting that it can undergo larger deformation before structural breakdown. This combination indicates a softer and more deformable bolus, which may facilitate oral deformation and propulsion during swallowing. Honey represents an intermediate condition, balancing flow control with manageable deformation. Pudding provides the greatest structural stability, the highest elasticity, and the highest cohesiveness, but this comes with greater firmness and adhesiveness, which may demand more oral and pharyngeal work and could increase residue risk.
Swallowing is a complex process involving compression deformation of food in addition to flow. Foods designed for dysphagia are carefully designed for safe swallowing. A primary descriptor is viscosity but additional rheological measurements such as shear, oscillatory, and axial stress measurements provide valuable insight into the functional performance of dysphagiaoriented foods. This work demonstrates the use of normal-forcerelated measurements to characterize bolus behavior under conditions relevant to swallowing:
- Nectar, honey, and pudding showed a progressive increase in viscosity, elasticity, and structural strength.
- Normal forces provided relevant information beyond viscosity, highlighting differences in bolus cohesiveness under flow.
- Tack measurements confirmed higher extensional resistance and structural integrity for honey and pudding than for nectar.
References
- Nishinari K, Turcanu M, Nakauma M, Fang Y. Role of fluid cohesiveness in safe swallowing. npj Sci Food. 2019;3:5.
- Hadde EK, Chen J, Zhao Y. The Importance of Extensional Rheology in Bolus Control during Swallowing. Sci Rep. 2019;9:16130.
Acknowledgement
For more information or to request a product quote, please visit www.tainstruments.com to locate your local sales office information.
This paper was written by Carlos Gracia Fernández, Principal Applications Scientist.
TA Instruments and Discovery are trademarks of Waters Corporation or its affiliates.
Click here to download the printable version of this application note.