Keywords: Rheology, Tribology, TGA, Rheo-IS, Chocolate
RH175
Abstract
The texture, mouthfeel, stability, and sensory perception of chocolate is governed by complex interactions among fat phases, dispersed solids, and interfacial structures. In this study, four commercially available chocolate formulations, including white, 100% dark, ruby, and Dubai-type chocolate, were characterized using an integrated approach combining rheology, tribology, thermogravimetric analysis (TGA), and Rheo-Impedance Spectroscopy (Rheo-IS).
The results revealed distinct structure-property relationships across the formulations. TGA differentiated thermal stability and decomposition pathways associated with compositional complexity. Rheological measurements showed that ruby chocolate exhibited the highest viscosity and strongest thixotropic recovery, indicating a highly rebuildable microstructure, while 100% dark chocolate displayed low viscosity and limited structural recovery consistent with a predominantly melted cocoa matrix. Tribological measurements linked these structural differences to lubrication behavior relevant to oral processing, with white chocolate exhibiting the lowest friction at high sliding speeds. Rheo-Impedance measurements provided additional insight into microstructural organization and heterogeneity, revealing high electrical resistance for 100% dark chocolate, strong shear- and temperature-dependent behavior for ruby chocolate, and exceptionally high polarization responses for Dubai-type chocolate arising from its complex multiphase composition.
Together, these complementary techniques provide a comprehensive framework for connecting formulation composition with thermal, mechanical, tribological, and dielectric properties. The results demonstrate the unique value of Rheo-Impedance Spectroscopy as a sensitive tool for probing microstructural organization and reveal how advanced characterization can support the design of chocolate products with targeted texture, mouthfeel, and consumer experience.
Chocolate is a complex multiphase material consisting of cocoa butter, cocoa solids, sugars, milk-derived ingredients, and other dispersed components. Its processing, stability, texture, and sensory properties are strongly influenced by the interactions between these phases. The microstructure of chocolate affects not only flow behavior during manufacturing but also mouthfeel and consumer perception [1, 2].
Thermal analysis techniques such as thermogravimetric analysis (TGA) provide information regarding formulation complexity and compositional differences through the identification of decomposition pathways and thermally stable fractions. However, thermal methods do not directly probe microstructural organization or interfacial interactions. Rheological characterization has long been used to evaluate chocolate processing performance and structural behavior. Measurements such as viscosity, viscoelasticity, and thixotropic recovery provide valuable information regarding particle interactions, fat phase mobility, and network formation. However, rheological measurements alone are often insufficient to fully describe the complexity of chocolate microstructure [1, 2].
Tribology has emerged as an important complementary technique for understanding oral processing and sensory perception. Friction measurements under conditions relevant to oral lubrication provide insight into creaminess, smoothness, and particle entrainment effects. While rheology describes bulk flow behavior, tribology characterizes the interactions occurring at contacting surfaces during consumption [3].
Rheo-Impedance Spectroscopy represents a promising but relatively unexplored approach for chocolate characterization. By monitoring resistance, reactance, and capacitive behavior, dielectric measurements can probe charge transport, polarization mechanisms, and interfacial phenomena within complex food matrices. When combined with rheometry, Rheo-IS enables the investigation of structural changes induced by shear and temperature.
The objective of this study was to investigate the relationships between rheological, tribological, thermal, and dielectric properties in four commercially available chocolates: white, 100% dark, ruby, and Dubai-type chocolates. By combining these complementary characterization methods, the study aims to reveal how formulation complexity influences microstructural organization, lubrication behavior, and thermal stability.
White chocolate, 100% dark chocolate, ruby chocolate, and Dubai-type chocolate (referred to as DTC in this work) were selected as representative chocolate products with distinct compositions and structures. White chocolate is primarily composed of cocoa butter, sugar, and milk solids, while 100% dark chocolate contains only cocoa-derived ingredients without added sugar. Ruby chocolate is produced from specially selected cocoa beans and is characterized by its natural pink color and fruity flavor profile. DTC chocolate consists of a chocolate shell filled with a pistachio-based cream and crispy kataifi pastry, resulting in a more complex multiphase structure. All samples were purchased from premium commercial brands.
A Waters TA Instruments™ Discovery™ HR 30 Rheometer (Figure 1) and a Waters TA Instruments Discovery TGA 550 (Figure 2) were used for all measurements. The HR 30 is a versatile rheometer capable of accommodating multiple accessories, enabling characterization of the rheological, tribological, and dielectric properties of chocolate samples. All rheological, tribological, and Rheo-Impedance measurements were conducted at 37 °C to approximate physiological conditions during oral processing. The following experiments were conducted in TRIOS™ Software:
Thermogravimetric Analysis (TGA)
- Sample mass: Approximately 25 mg
- Temperature range: Room temperature to 800 °C
- Heating rate: 10 °C/min
- Atmosphere: Air
- TGA pan type: Platinum 100 μl
Rheology (40 mm crosshatched parallel plate, 1 mm gap)
- Three-step thixotropy test:
- Step 1: 0.01% strain amplitude (within the linear viscoelastic region)
- Step 2: 10% strain amplitude (outside the linear viscoelastic region)
- Step 3: 0.01% strain amplitude (structural recovery)
- Flow curve: Shear rate ramp from 100 s⁻¹ to 0.01 s⁻¹
Rheo-Impedance (40 mm parallel plate, 1 mm gap)
- Rheo-Impedance flow sweep:
- Shear rate: 100 s⁻¹ to 0.001 s⁻¹
- Applied voltage: 1 V
- Dielectric frequency range: 4 Hz to 8 MHz
- Rheo-Impedance flow transient (cooling down from 37 °C to 25 °C):
- Constant shear rate: 1 s⁻¹
- Applied voltage: 0.5 V
- Fixed dielectric frequency: 1000 Hz
Tribology (Waters TA Instruments Ball-on-Three-Plates geometry)
- Stribeck curve measurements
- Axial force: 2 N
- Angular velocity: 0.001 to 40 rad/s
The applied normal force was selected to approximate tongue-palate contact conditions encountered during oral processing.

Figure 1. Waters TA Instruments Discovery HR 30 Rheometer with a) Rheo-IS Accessory and b) Ball-on-3 Plates Tribology Accessory

Figure 2. Waters TA Instruments Discovery TGA 550
Figure 3 presents the TGA profiles of the four chocolate samples under an air atmosphere. Although all samples exhibited multistep thermal degradation behavior, notable differences were observed in both the onset of decomposition and the stability of intermediate decomposition products, reflecting differences in formulation and composition.

Figure 3. Thermogravimetric (TGA) profiles of the four chocolate samples under an air atmosphere
The first region (< 200 °C) showed minimal weight loss for all samples, indicating low moisture content and good thermal stability within temperatures relevant to storage, processing, and consumption. Only minor losses associated with residual volatiles were observed.
The second region (approximately 200 to 350 °C) corresponded to the decomposition of sugars, milk solids, and other lower-molecular-weight organic constituents. White, ruby, and DTC chocolates began to lose mass earlier in this region, while the 100% dark chocolate exhibited a noticeable shift toward higher decomposition temperatures. This behavior is consistent with the composition of 100% dark chocolate, which consists primarily of cocoa-derived materials and lacks the significant sugar- and milk-based components present in the other formulations. As a result, the 100% dark chocolate demonstrated the highest onset thermal stability among the samples studied.
The third region (approximately 350 to 450 °C) was characterized by rapid decomposition and oxidation of carbonaceous materials formed during the earlier degradation stages. The 100% dark chocolate showed the steepest mass-loss event in this temperature range. While this sample exhibited the highest resistance to initial decomposition, once degradation began, the large concentration of cocoa solids produced carbon-rich intermediates that were rapidly oxidized under the air atmosphere. Consequently, the mass decreased sharply as these materials were converted to gaseous products.
Above approximately 450 °C, oxidation of the remaining carbonaceous residues became the dominant process. Interestingly, ruby and DTC chocolates retained substantially more mass than either white chocolate or 100% dark chocolate throughout this region. For the DTC chocolate, the pistachio filling and kataifi pastry introduced additional carbohydrates, proteins, and complex organic components that may have contributed to the formation of stable carbonaceous residues during thermal degradation. Similarly, ruby chocolate appeared to generate intermediate decomposition products that persisted to higher temperatures before complete oxidation occurred. Although the exact mechanisms cannot be determined from TGA data alone, both formulations exhibited greater resistance to oxidation in this temperature range than either white chocolate or 100% dark chocolate.
To further investigate the decomposition mechanisms, derivative thermogravimetric (DTG) curves were generated for the 100% dark chocolate and compared with those of the ruby and DTC chocolates (Figures 4 and 5). The DTG curves reveal several overlapping degradation events that are less apparent in the mass-loss curves.
The 100% dark chocolate exhibited a dominant and relatively narrow DTG peak centered near 380 °C, indicating that most of the thermal degradation occurred over a limited temperature range. This observation supports the sharp mass-loss event observed in Figure 3 and is consistent with a composition dominated by cocoa-derived materials. Once decomposition began, the resulting carbonaceous intermediates were rapidly oxidized, leading to the pronounced DTG peak and rapid reduction in mass.

Figure 4. DTG curves comparing ruby chocolate and 100% dark chocolate

Figure 5. DTG curves comparing DTC chocolate and 100% dark chocolate
In contrast, both ruby and DTC chocolates displayed multiple degradation peaks distributed across the temperature range. An initial peak near 230 °C is consistent with degradation of sugar-rich and milk-derived components, while broader events between approximately 280 and 380 °C correspond to decomposition of cocoa butter and other organic constituents. These multiple degradation events reflect the greater compositional complexity of the ruby and DTC chocolate formulations compared with the simpler composition of the 100% dark chocolate.
A notable feature of both ruby and DTC chocolates is the presence of an additional DTG peak near 500–530 °C. This peak corresponds to the oxidation of carbonaceous residues formed during earlier decomposition stages and explains the higher residual mass observed in Figure 3 above 400 °C. The delayed oxidation behavior suggests that these samples generate more thermally stable intermediate decomposition products than either white chocolate or 100% dark chocolate. The effect is particularly pronounced for the DTC chocolate, likely due to the contribution of the pistachio filling and kataifi pastry, which introduce additional organic components capable of forming stable char structures during thermal degradation.
Overall, the TGA results and these compositional differences provide valuable insight into the structural complexity of the samples and establish a foundation for interpreting the rheological, tribological, and Rheo-Impedance results discussed in the following sections.
Rheological measurements were performed at 37 °C to approximate physiological conditions encountered during oral processing. Figure 6 presents the flow curves of the chocolate samples, while Figures 7 and 8 show the three-step thixotropy results for ruby and 100% dark chocolate, respectively.

Figure 6. Flow curves of white, ruby, and 100% dark chocolate measured at 37 °C
From a consumer perspective, the higher low-shear viscosity of ruby chocolate suggests a thicker mouthfeel during the initial stages of melting in the mouth. At higher shear rates, representative of tongue movement and swallowing, the viscosity differences become less pronounced as all samples exhibit significant shear thinning, facilitating oral processing.
These differences suggest that the rheological response is governed not only by the liquid fat phase but also by the concentration and interactions of suspended particles. In addition to cocoa-derived components, ruby and white chocolates contain sugar, milk solids, and other particulate ingredients that increase the effective solids loading and promote particle-particle interactions. Consequently, these formulations behave as more concentrated suspensions and exhibit higher viscosities than the 100% dark chocolate.
To further investigate structural breakdown and recovery, three-step thixotropy experiments were performed. In these tests, the samples were first characterized within the linear viscoelastic region (0.01% strain), followed by application of a large deformation (10% strain) to disrupt the structure. Recovery was then monitored at 0.01% strain.

Figure 7. Three-step thixotropy results for ruby chocolate

Figure 8. Three-step thixotropy results for 100% dark chocolate
The most notable difference between the two samples is their ability to recover after structural breakdown. Following exposure to the high-strain interval, ruby chocolate exhibited a gradual but substantial increase in both G′ and G″ during the recovery step, indicating that the disrupted microstructure was progressively rebuilt over time. In contrast, the 100% dark chocolate showed only limited recovery, with both moduli remaining significantly below their initial values throughout the experiment. The ruby chocolate demonstrated a much greater degree of thixotropic recovery, suggesting a reversible microstructure and a stronger ability to reform structural networks after deformation. Based on the storage modulus (G′), the ruby chocolate recovered to approximately 100% of its initial value after 1000 s, indicating nearly complete structural recovery. In contrast, the 100% dark chocolate recovered only about 17% of its initial storage modulus.
The differences observed in both viscosity and recovery behavior suggest that the extent of structural organization remaining at 37 °C differs among the chocolate formulations. While 37 °C is above the typical melting range of cocoa butter, ruby chocolate may retain residual fat-crystal structures and particle networks arising from their more complex compositions, which include sugar, milk solids, and milk-fat-derived components. These residual structural elements can act as structural templates that facilitate network reformation following deformation.
In contrast, the 100% dark chocolate appears to behave more like a fully melted suspension of cocoa particles dispersed within a liquid fat phase. Consequently, once the structure is disrupted during the high-strain interval, fewer structural elements remain available to facilitate network reformation, resulting in a lower degree of thixotropic recovery.
Tribological measurements were performed using a Ball-on-Three-Plates geometry at 37 °C to approximate oral processing conditions. Figure 9 presents the coefficient of friction vs. sliding speed for the white, ruby, and 100% chocolate samples.

Figure 9. Friction curves of white, ruby, and 100% dark chocolate obtained at 37 °C
At low sliding speeds, the 100% dark chocolate exhibited the lowest friction coefficient, while ruby and white chocolates showed slightly higher friction values. The lower friction of the 100% dark chocolate is consistent with the rheological results, which indicated that this formulation behaves as the least structured system at 37 °C and is therefore able to form an effective fat-rich lubricating layer between the contact surfaces. White and ruby chocolates exhibited moderately higher friction, likely reflecting the presence of additional suspended components such as sugar and milk solids that can influence surface interactions.
As the sliding speed increased, ruby chocolate maintained the highest friction coefficient while the 100% dark chocolate continued to exhibit the lowest friction. This behavior agrees well with the rheological measurements, where ruby chocolate showed the highest viscosity and thixotropic recovery. Together, these results suggest that the more structured microstructure of ruby chocolate contributes to increased resistance to motion under lubricated contact conditions.
The most notable feature of the tribological data is the crossover observed at high sliding speeds. At the highest sliding speeds, however, a crossover in friction behavior was observed. The friction coefficient of the 100% dark chocolate increased rapidly and eventually exceeded that of ruby chocolate, while white chocolate exhibited the lowest friction. This transition suggests a shift from fat-dominated lubrication toward particle-influenced lubrication. Although the abundant cocoa butter in the 100% dark chocolate promotes effective lubrication at low and intermediate speeds, the high concentration of cocoa solids becomes increasingly important at higher entrainment speeds, where particle-fluid interactions contribute to increased friction. In contrast, the absence of cocoa solids in white chocolate enables the formation of a smoother lubricating film, resulting in the lowest friction in the high-speed regime.
From a sensory perspective, the tribological results suggest that ruby chocolate, with its consistently higher friction and stronger structural recovery, is expected to provide a thicker, and more persistent mouth-coating sensation. White chocolate behaves somewhat differently, exhibiting higher friction initially but the lowest friction at high sliding speeds, which may contribute to a creamy and smooth sensation during later stages of oral processing.
Electrical measurements provide insight into charge transport and polarization processes occurring within the chocolate microstructure. Because the dielectric frequency was varied over several decades, the Rheo-Impedance response probes electrical phenomena occurring over different time and length scales. High frequencies primarily probe local charge motion and short-range polarization, while low frequencies are increasingly sensitive to long-range charge transport and interfacial polarization throughout the material. Figure 10 shows the frequency dependence of the series reactance (Xs) for the different chocolate formulations.

Figure 10. Frequency dependence of series reactance (Xs) for the chocolate formulations during flow
The most distinctive response was observed for the DTC chocolate, which exhibited substantially higher reactance values than all other formulations. The difference became particularly pronounced at low frequencies, where reactance increased dramatically relative to the other chocolates.
Reactance reflects the ability of the material to store electrical energy through polarization processes. The high reactance observed for the DTC chocolate suggests extensive charge accumulation and interfacial polarization within the sample. This behavior is consistent with the highly heterogeneous composition of DTC chocolate, which contains chocolate, pistachio filling, kataifi pastry, sugar-rich regions, protein-containing components, and multiple fat-rich domains. The numerous interfaces created by these components provide abundant sites for polarization, resulting in the strongest dielectric response among all formulations.
Figure 11 shows the frequency dependence of the series resistance (Rs) for the different chocolate formulations.

Figure 11. Frequency dependence of series resistance (Rs) for the chocolate formulations during flow
White chocolate exhibited the lowest resistance, together with minimal shear-rate dependence. Unlike the 100% dark chocolate, white chocolate contains sugar and milk solids. These components appear to create a more electrically accessible microstructure that facilitates charge movement and redistribution. The compact cluster observed in the plot indicates a comparatively homogeneous system with limited structural evolution during deformation.
While Figures 10 and 11 independently highlight polarization and charge-transport behavior, the Nyquist representation shown in Figure 12 combines both responses into a single visualization, enabling direct comparison of the electrical signatures of ruby and 100% dark chocolate.

Figure 12. Nyquist representation of the Rheo-Impedance response for 100% dark and ruby chocolate during flow
The Nyquist plot reveals distinct electrical signatures for the two formulations. The 100% dark chocolate reached higher resistance values in the low-frequency region, indicating more restricted long-range charge transport throughout the microstructure. In contrast, ruby chocolate exhibited a stronger dependence on both frequency and shear rate (Figures 11 and 12), producing a broader distribution of responses. Looking at the Nyquist plot, the 100 s⁻¹ ruby chocolate dataset clearly deviates more from the lower shear-rate datasets than the 100% dark chocolate datasets do. The higher low-frequency resistance of the 100% dark chocolate likely reflects its cocoa butter-rich insulating matrix and the absence of milk-derived components, resulting in fewer pathways for long-range charge transport compared with ruby chocolate.
This increased sensitivity suggests that the ruby chocolate microstructure continuously reorganizes during deformation. Interestingly, this observation parallels the rheological measurements, where ruby chocolate exhibited the strongest thixotropic recovery. The agreement between the rheological and electrical measurements suggests that the same structural features responsible for mechanical rebuilding also influence charge transport and polarization.
Figure 13 compares the Rheo-Impedance response of ruby and 100% dark chocolate during cooling from oral processing (37 °C) to room temperature (25 °C) at a constant shear rate of 1 s⁻¹ and a fixed dielectric frequency of 1000 Hz.

Figure 13. Effect of temperature on the Rheo-Impedance response of 100% dark and ruby chocolate measured at 1000 Hz.
Cooling produced negligible changes in either resistance or reactance for the 100% dark chocolate, indicating that the local electrical microstructure remained largely unchanged over this temperature range.
In contrast, ruby chocolate exhibited measurable increases in both resistance and reactance as the temperature decreased from 37 to 25 °C. The increase in resistance indicates that local charge transport becomes progressively more restricted during cooling, while the simultaneous increase in reactance suggests stronger polarization within the microstructure. Together, these observations indicate that cooling promotes increased structural organization and modifies the electrical interactions occurring at existing interfaces.
The fact that these changes are observed even at 1000 Hz demonstrates that the evolving structure affects not only long-range transport pathways but also local dielectric environments and short-range polarization mechanisms. This interpretation is consistent with both the rheological measurements and the frequency-sweep Rheo-Impedance results, further supporting the conclusion that ruby chocolate possesses a more dynamic and responsive microstructure than the 100% dark chocolate sample.
From a formulation perspective, the Rheo-Impedance results provide insight into microstructural organization, stability, and complexity. White chocolate exhibited the lowest resistance, suggesting the most electrically accessible and homogeneous microstructure. The 100% dark chocolate showed high low-frequency resistance and minimal sensitivity to shear and temperature, indicating a stable microstructure with restricted long-range charge transport. Ruby chocolate displayed the strongest sensitivity to shear, temperature, and frequency, revealing a dynamic microstructure capable of continuous reorganization. DTC chocolate exhibited exceptionally high reactance values and the strongest polarization response, highlighting its highly heterogeneous composition and extensive interfacial structure. Collectively, these results demonstrate that Rheo-Impedance measurements can differentiate formulation uniformity, microstructural stability, and dielectric complexity while providing information complementary to conventional rheological characterization.
This work demonstrates that the combination of TGA, rheology, tribology, and Rheo-Impedance provides a powerful framework for differentiating chocolate formulations and uncovering microstructural features that cannot be captured by any single analytical technique alone. By linking thermal behavior, mechanical response, lubrication performance, and electrical properties, these complementary methods provide a more complete understanding of the relationships between formulation, structure, processing, and performance.
Despite all being chocolate-based systems, the four formulations exhibited distinctly different behaviors. The 100% dark chocolate displayed the most stable microstructure, characterized by low viscosity, limited structural recovery, restricted long-range charge transport, and minimal sensitivity to shear or temperature. In contrast, ruby chocolate exhibited the thixotropic recovery and the greatest sensitivity to shear, temperature, and dielectric frequency, indicating a highly dynamic microstructure capable of continuous reorganization. White chocolate showed the lowest resistance and the simplest lubrication and dielectric behavior. DTC chocolate exhibited by far the strongest polarization response, reflecting the dielectric complexity expected from its highly heterogeneous multiphase composition.
These measurements also provide a scientific basis for sensory differences that consumers readily perceive. The cleaner melt profile of the 100% dark chocolate is consistent with its simpler and more stable microstructure, whereas the higher viscosity and stronger structural rebuilding observed in ruby chocolate help explain its more persistent mouth-coating sensation. Likewise, the distinctive character of DTC chocolate can be associated with the numerous interfaces and structural domains created by the combination of chocolate, pistachio filling, and kataifi pastry.
By translating sensory observations into quantifiable thermal, mechanical, tribological, and dielectric properties, this integrated approach provides formulators with actionable information for designing products with targeted texture, mouthfeel, stability, and consumer experience. As food formulations become increasingly complex, combining Rheo-IS with established characterization methods offers a promising strategy for accelerating product development and gaining deeper insight into structure-function relationships.
References
- S. T. Beckett, M. S. Fowler and G. R. Ziegler, “Beckett’s industrial chocolate manufacture and use,” John Wiley & Sons, 2017.
- E. O. Afoakwa, “Chocolate science and technology,” John Wiley & Sons, 2016.
- X. Wang and J. Chen, “Food oral processing: Recent developments and challenges,” Current Opinion in Colloid & Interface Science, vol. 28, pp. 22–30, 2017.
Acknowledgments
For more information or to request a product quote, please visit www.tainstruments.com to locate your local sales office information.
This paper was written by Behbood Abedi, Ph.D. and Karim Elhattab, Ph.D., Applications Scientists at Waters Corporation.
Waters, TA Instruments, Discovery, and TRIOS are trademarks of Waters Corporation or its affiliates.