UV LIGHT GUIDE


A Smart Swap™ accessory for rheological characterization of UV curable materials is available for the DHR-3 and DHR-2 rheometers. The accessory uses a light guide and reflecting mirror assembly to transfer UV radiation from a high-pressure mercury light source. The UV Light Guide accessory is configured using a lower Smart Swap assembly with light source mount, collimator, and 5 mm light guide. A UV light source (Exfo Omnicure S2000), with wavelengths in the range of 320 to 500 nm, and triggering cable are optional.